Curated with aloha by
Ted Mooney, P.E. RET

The authoritative public forum
for Metal Finishing 1989-2025

Archives of the finishing.com Hotline
Topics/Threads 35000 to 35999
The finishing.com Hotline includes more than 60,000 Shop Problems, Q&A's and RFQs about metal finishing. This page is an archive of a thousand of those discussions. You may prefer to start at our Home page, view the most recent threads, or search the site.

35002. Titanium anode passivation
35005. Adhesion/Bond strength of hard chrome deposits in various type of bath
35006. Suitable sodium nitrite levels to inhibit corrosion
35007. Polishing of surgical instruments made out of SS410
35014. 304L discoloration based on temperature data
35018. Need a chromated Anti tarnish treatment for Silver plated parts
35020. Question about size of the international electroplating industry
35021. Glass Fibre Canoe Refinishing
35023. Estimating levels of hexavalent chromium in plated metal parts
35024. Powder Coating Aluminum Racing Rims
35025. Tin electroplating
35026. What materials (chemicals) are used for electroplating zinc-zamac
35027. Dull and black SS media
35028. Need Photocopier Drum Coating
35030. Electrocoagulation research
35032. DM water plant
35033. I would like to know a procedure the best way for test pH of DI water
35034. Coating Adhesive onto small parts and steel wire
35035. Can Zn/Co alloy plating withstand corrosion resistance
35036. How to remove manganese (Mn) and magnesium (Mg) from nickel sulphate solution ?
35037. Plating of narrow areas
35038. Stainless steel electropolishing
35039. Sa 2.5 norms
35040. Boron in Demineralized water as a corrosion prevention solution
35041. Chroming plastic parts for the food industry
35044. Wastewater treatment
35045. Restoring patina on pewter
35047. I have an allergic reaction to my 10 karat white gold wedding ring
35048. Kawasaki aluminum air cooled head
35049. JS500 vs Dacromet
35050. Plating fused silica fiber
35051. Effect of high boron on lime consumption in Fluoride precipitation process
35052. Measuring Evaporation Rate by ALOHA software
35053. How to create a diamond abrasive surface on a metal strip
35056. Electroless Ni-P-SiC composite coating
35059. Passivation as per PS-231900 type II
35060. Glossy black finish on carbon steel
35063. DISCOLORATION DURING DURING H950 HEAT TREAT
35064. Salt spray test failure as per ASTM B117
35065. Electrically Insulating a Cast Metal Part
35066. EN Porosity Test with Copper sulphate
35067. Spot test on clear chem-film
35068. What is the difference between electroplating and conversion coating?
35069. Galvanizing not qualifying in salt spray test
35070. Plating of Spanker Tip for Soft Solder
35071. Need chemical compositions of Electrolytic chrome plating
35072. Free cutting steel coating by electrodeposition
35073. Brass entry set discoloration
35074. What is the best way to heat a galvanized steel "hot tub" without causing any damage to it?
35075. Intergranular and transgranular crack in 17-4PH
35076. Aluminum Anodizing and RoHS compliance
35077. RAL or PMS equivalent to FED-STD-595 13538
35078. Guarantee on PVDF Coatings
35079. Potassium Permanganate vs Sodium Permanganate for coloring architectural aluminum
35080. Fluorine retention on anodized aluminum surfaces
35081. Anodize thickness
35082. Acid based electrolytic cleaning
35083. Removing magnetism from stainless steel 304
35085. Yellow mark during Line stop in Pickle Process
35086. Plating defect after crimping
35087. Galvanising - Top Dross
35088. Trivalent finish for aluminum
35092. STABILITY OF H2O2 IN QAC's
35094. Carbon steel corrosion in aqueous ammonia high temperature system
35095. AA, ICP, ICP-MS
35097. Painting over powder coated aluminum
35098. SS 304-2B 22Gage - can rust occur in a water storage application?
35110. Metalizar un plastica se basa
35113. Using 17-4 PH stainless steel for wood lathe turning tools
35114. Can you paint a car with house paint
35115. Porosity problem in cast iron
35117. What is zinc dichromate type II class 3?
35118. PP Compatibility With Chromic Acid Solutions
35119. Ways to color brass cartridges
35121. Metal contamination analysis in chrome
35122. Contamination Black spots on machined 7075-T73 Aluminum
35125. Blue pitting on the downward surface After Electropolish
35126. Powder Coating Porosity Related to Metal Pretreatment
35127. Corrosion Resistant Coating for Steel
35130. Zinc as electrolyte produces slow results. How can I speed up the process?
35132. In need of hard non-magnetic material
35133. Cleaning cement from copper utensils
35135. Aging new zinc counter top
35138. Alodine and/or Zinc Chromate Conversion Coating Needed for Homebuilt Aluminum Airplane?
35139. Painting plastic
35141. SCRATCHES ON A WALL MIRROR
35142. Powder Coated Rusted Steel roofing
35143. How to Darken Polished Brass Finish
35144. Smith and Wesson gun blueing ?
35145. Chemically removing copper color from Brass improperly cleaned with HCL
35146. Titanium finishing - how do I polish?
35148. Titration for acid with Ni and Ti present
35149. Photopolymer processing
35153. Chemically removing organics
35154. Painting kevlar fabric impregnated with phenolic/PVB resin
35156. Safety of engineered wood flooring
35162. Red striations on "cleaned" brass
35163. Repeat Nitrocarburizing
35164. Boehmite as detackification agent for paints
35165. Electroless Plating Compatible with Sulfur
35168. Iron phosphating conversion layer over a galvanized steel (spray system)
35172. Chemical compound for removing the plastic or rubber coating on copper wire
35174. Why dilute sulfuric acid with vinegar for electroplating?
35175. Cadmium plating of 4130 condition N steel round .049 wall tubing
35176. Varnishing wood windows - in and out
35178. Preparation for Kool Sealing NEW galvanized tin
35182. Halt cyanide gold stripper action prior to plate out
35184. Hard chrome plating catalyst
35186. Platinum Q Salt Plating
35187. Electropolishing
35188. Stainless steel cleaning with H2O2
35189. Matte black finishes for steel
35191. How to brighten galvanized finish on metal
35194. Black chrome
35195. Why is white gold ring yellow not silvery?
35196. Removing spray paint from powder coated surface
35197. Questions about zinc electroplating specification Fe/Zn8, thicknesses and chromate post-treatments
35199. Lead and arsenic poisoning
35200. How durable can Chrome/Steel electroplated ABS get ?
35201. Acid Zinc sulphate throwing power additives - need info
35202. QQ-S-365 Type 2 Grade A Silver plating
35204. Passivation ASTM A967 Type II leaves yellow or brown spots on 304
35205. Chemical cleaning a dark deposit from surface of aluminium engine block casting
35206. Aluminum 5052 & Type of Fasteners
35214. Need to determine carbonates in cadmium plating solution using autotitration
35217. Electroless plating of Platinum
35219. Titanium plating with Ni bath
35222. Re-Machining of part that has been passivated to ASTM A967
35223. What does the finish requirement 63 RMS mean?
35224. Coating for heat exchanger tube ID
35225. Coating Threads For Lens Repair
35226. I want to buy rhodium where do I get it
35227. Contamination and Foreign Material on Copper
35230. Coating alloys on rough sapphire substrates
35231. Finishing Brass Doorknobs and Locksets
35232. Clear coat sealer for cast iron fountain
35234. Voltages required to plate various metals
35237. Poor adhesion of waterbased paint on acrylic solvent based primer coat
35239. Mill finish vs. anodized extruded aluminum product
35240. How to increase nickel stamper hardness
35242. Cold acid formulation please
35255. Distilled water for sulfamate bath?
35256. Problems with the Ni-P equilibrium phase diagram
35257. Converting from Cyanide to Alkaline base on Zinc Plating
35258. Alternate Hard Chrome Mixed Catalyst
35260. Residual current of anodizing tank
35261. How to Reduce Zn phosphate spray type coating weight?
35263. Painting fiberglass bathtub
35265. Poor adhesion of Pure Tin Plating on copper strip
35270. Help with Zinc-Nickel per AMS2417 Type 2
35271. Sealing 45% Chromic Acid
35272. Hot water Seal vs Nickel Acetate Seal
35273. RE-PLATING OF PLATED PARTS
35274. Painting of Mn-Phosphated Surfaces
35277. On average, how long can brass stay totally submerged in water?
35280. How am I going varnish rusted steel?
35281. Galvanized shackle to stainless steel for saltwater buoy
35283. Plating inside a tube
35284. Looking for a source for oil rubbed finish restorer
35285. Spray painting Aluminum
35286. Uneven thickness of Au/Ni bonding pads
35287. Inert anode material for nickel refining
35288. Minimising copper in alkaline phosphate gold bath
35289. Pulse Plating of Chrome
35291. Copper corrosion caused by potassium or sodium chloride water treatment
35292. What's the maximum corrosion resistance coating for bolts?
35296. Quantitative Analysis of Au in spent plating baths
35302. I wish to remove paint from lead on stained glass windows
35303. Getting rid of the gold plating on hardware
35304. Making a sword
35306. Can Zinc Plate, Class 12 Type 2, Bronze or Olive Drab in Color be applied to Chain Link in accordance with ASTM B695
35317. Can I apply a Mirror effect on plastic?
35318. Performance of various pickling solution for rusty mild steel
35319. Remove the zinc phosphate
35320. Cheap Imitation Jewelry
35321. My chrome motorcycle rims are of gold/ yellow tint doesn't match?
35323. Deflash Solution Concentration
35326. Specs needed chrome plating ABS plastic automotive exterior
35328. PASSIVATION -- Chelant Passivation Chemicals or Nitric Acid ?
35329. Sanding aluminum sheets and tubing
35330. HCr Galvanic Corrosion Alternate?
35331. Floc coating of filters
35332. VOIDS on Solder Die Bonding
35338. Chrome(Cr6) free finishing in European Markets
35339. QQ-Z-325
35340. Ni/Cr coating thickness
35341. Silver plating adhesion problem
35342. White patches in Chrome Plating
35343. Prevention of corrosion on new SS lines and vessels
35345. Stainless steel 202 grade finishing
35349. My GCSE Project: protecting candle holder from rust
35350. Concentration of cell EMFs
35352. RoHS compliant Plating to replace Bright Blue Zinc Type II Class III
35354. Galvanizing Problem
35356. Electroforming on glass
35357. Surface coatings for titanium
35359. Stainless steel oxidation
35360. Stainless Steel Flat Stove Top Damage (HELP!)
35361. Has anyone had any luck with non-cyanide copper strikes?
35366. Titanium Electropolishing
35367. Porous inert electrodes
35368. Stripping of Copper Leaving Nickel unchanged
35370. Copper aging
35371. Coloring Damascus Steel
35372. New Stainless Rusting
35373. Flexible spray chrome
35376. Durable high-gloss clear coat finish for painted titanium golf clubs
35377. Trying to figure out amp hours to the rate of copper electroplated
35379. Etching magnesium plates for hot stamping ribbons
35380. What is Pickling Process?
35381. Buffing and polishing
35384. Strainer for zinc chrome
35387. Rust on chrome
35395. Correlation of salt spray method and humidity test
35398. Release problems in CD molding
35399. Want dull zinc and gold passivation
35401. PVDF LINED TANKS
35403. Thin layer of glass coatings or ceramic coatings on polycarbonate lens
35405. Copper/Aluminum interaction
35406. Masking
35407. Protecting 300 stainless from muriatic acid
35413. Cleaning a sheet of copper
35415. Size of polishing particles vs. roughness of finish
35417. How do I bring the sheen back to the lead in leaded windows?
35418. Platinum ring
35419. Horizontal scrubber design
35420. Cyanide treatment inconsistency
35421. Are brass valves suitable for DI Water?
35422. Is ASTM B-117 done pre-assembly or post?
35423. Hard chrome plating - stripping
35424. Orange peel problem
35425. Zn coated conduit white rusted in sea voyage
35426. Titanium coating of OEM motorcycle wheels
35427. How to satinize aluminum
35428. What mold coating is best for molding Polyurethane foam?
35429. Blistering between copper-nickel
35434. Mils to Microns
35435. 100 yr old coppper patina removal for solderability
35436. Refrigerator repair
35441. REPAIR OF WORN BORE IN 17-4PH Part
35442. Rusting, corroded 316 stainless steel chain
35444. Polishing/finishing bearing races and housings
35446. Need bead blasting equipment and media
35447. Plastic or Titanium Clip
35448. Zn Plating on Steel Based Spring
35449. Mould texturising
35450. Low Friction Coefficient
35451. Wire hot dip galvanizing
35453. Stains on a copper roof
35454. Aluminum boat in salt water
35456. Salt-spray comparison of RoHS compliant Steel finishes
35458. What alternatives are available for Chromate Coatings?
35470. RoHS restrictions on Hexavalent Chromium
35471. Ozone+UV destruction of Cyanides
35472. Treatment of cyanide in wastewater
35475. Repairing clearcoat on scratched polished alloy wheel
35476. Orange Peel measurement
35477. Thin glass coating or transparent ceramic coating for abrasion resistant purpose
35480. Zinc plating and rust
35492. Sodium Carbonate in Sodium Hypochlorite
35494. Cataphoretic coating of zirconium on tungsten
35495. Lead shot ballast in an aluminium yacht hull
35496. Powdercoating wheels to take out the flash
35498. What do I use to paint outdoor aluminum furniture
35499. Getting paint from "bleeding" shutters off our exterior brick surface
35501. Silver solder and chroming compatibility
35502. Fish-safe painting of a fiberglass fishpond
35503. Painting a blue color onto stainless steel
35505. Want to get lower zinc thickness by higher line speed
35507. Recovering silver via electroplating thum cell
35508. Potassium Dichromate Sealer
35515. Electroplating a key
35516. Constructing an Electrocoagulation Cell for School Project
35517. Is Electrophoretic coating an alternative to Galvanizing?
35520. What metal plating offers low thermal emissivity plus high temperature capability?
35521. Repairing deep scratch in clear lacquer table-top finish
35522. Performing electrolysis between H2O and Methyl Alcohol
35524. Will removing lacquer from trumpet leave the brass vulnerable to corrosion?
35525. What is TRICOAT or TRI-KOTE?
35526. What is Alumon plating?
35527. Health issues in welding on galvanized steel
35528. What is the difference between Cadmium & Zinc Plating
35529. Mask and de-mask solution
35531. Need a thin insulating coating for micro stainless steel housing
35538. Contractor needs to strip years of paint from copper gutters
35539. Clear coatings on bronze
35541. How to achieve a Black PVD finish
35542. Causes of defects in plated ABS
35543. Porosity problems in hard chrome plating
35545. Fading of Black Anodizing on heatsinks
35546. LM5 Alloy refuses to Anodize
35549. Is doing anodizing safe?
35550. Poor results from electroplating experiment
35551. What electrode can I use for electrolysis of water?
35554. PTFE degradation with water and heat
35556. Safety of chrome plated grilling surfaces
35557. Repainting a metal "girl" headboard
35558. Yellow gold diamond engagement ring is white in three weeks
35559. How to polish stainless steel beer kegs
35560. Terry cloth orbital polisher attachable to ordinary drill to polish chrome rims?
35561. Procedure for Homemade Fade Anodizing?
35562. copper sulphate (Crystal Blue) product killed my Koi. What now
35564. Re-sizing an Engineer's Iron Ring
35565. Can print maker prevent ink discoloration on etching plates?
35568. Want service to put matte finish on shiny stainless steel furniture
35570. Flame anodizing durability & controlled use of colours?
35572. Etch solution for A1050
35573. Acceptance criteria after salt spray test
35575. Fastening screw for circular saw is breaking
35576. Looking for best anti-tarnish agent for silver plated musical instruments
35582. Black corrosion on galvanized sheet metal
35584. I am new with a metal finishing supplier
35585. Gold migration or gold plating temperature resistance
35587. Process in decorative chrome plating
35588. Potential galvanic corrosion on Al camera parts
35589. Anodizing process question
35590. Hard Anodize on 6061-T6 Alum
35591. citric acid deoxidizing of aluminum?
35593. How to remove the oxide layer from Sn/Ag surface?
35594. API-610 requirement for combined mechanical and electrical run out
35595. Plating a vibration suppression device against high sodium water
35603. Need passivation chemical for brass plated articles
35607. Voids Resulting After The Reaction Of Nickel-plated Copper and Solder Paste
35608. Stainless steel Refrigerator scratches
35609. Conservator has questions on Bs 5493 repairs
35610. Removing chrome plating and nickel from aluminum valve covers
35611. Powder coat verus paint for fence
35613. Accumulation of Nickel salt in air agitation pipe
35614. Clearlyte deposition process
35615. Introduce me to the electorophoretic lacquer process please
35616. What makes for a better black oxide?
35618. Finger printing on Zinc & Clear passivate
35620. My Nickel anodes are getting black in bright nickel tank.
35621. Watts nickel strike analysis
35623. Clear Iriditing "burn off"
35625. Ammonium molybdate tetrahydrate as accelerator in iron phosphate
35626. DARK HEAT STAIN ON STAINLESS STEEL
35628. Electroless deposition of Ni on PET film
35630. Steel specification for battery contact
35631. Substrate cleaning using High pressure water jet
35632. Peeling Paint
35634. Cleaning aluminum screen enclosure frame
35635. High Current Density Leveler For Sulfamate Nickel?
35636. Evening tone of hot rolled steel
35637. Trying to clean some STUFF off my pipes
35639. Can you paint chrome legs on a table
35641. Painting brass shower fixture
35649. Boric acid control and what it does for nickel plating?
35650. How did we get from calling it kitchen zinc to sink?
35652. What is a pH sensor vs. a pH meter?
35653. Why do we have scratching on Zinc-Iron plating with black chromate?
35654. What maintenance program for Cu-Ni-Cr processes?
35655. Chromate conversion works in SS 316L fixtures but not PP barrels
35657. Alkaline Cleaning Agent versus Black Anodized Finish on Aluminum Heat Sinks
35658. Hard anodizing Aluminum with 1 mm thickness
35659. Want to electro etch stainless steel to smooth gray finish
35660. Speeds and feeds vs. surface finish
35661. Designing a zinc license plate frame to be chrome plated
35667. Sputter Coating Glass with Silver
35669. How to etch Niobium oxide from thin Niobium films
35670. Information on gold salvage, PLEASE!
35672. Looking for a GM and Chrysler finish spec equal to S424
35673. Website to change German material specs. to AISI?
35675. Big problem with PVD Titanium Nitride coating
35676. Nickel hydroxide causes problem in electroless nickel tank
35677. Protecting non aluminum metals when anodizing
35678. Chromating 6061 T6511
35679. Passivating SS Pipe
35684. Soldering the seams of a countertop laminated with .030 zinc sheet metal
35685. What should the chloride level be maintained at in cool towers?
35686. Stripping Hard Coat Anodize
35687. Chrome removal from aluminum wheels
35689. pH titration of weak acid with overlapping pKa values
35693. Gold Plating
35694. Welds turn black when clear anodized
35697. Carburetor re-coloring
35699. Dried-on Brasso removal
35700. Fire suppression equipment required in open faced spray booth using non-flammable powder
35702. Chrome Plating Free Machining Brass for Wear Purposes
35703. Polishing .040 aluminum sheet metal
35708. Specs for salt spray solution
35709. Painting Thickness
35710. Ebonol C50 on brass doorware
35711. Change of the kettle?
35712. CADMIUM PLATING ITS ILL EFFECTS ON THE ENVIRONMENT
35713. Convolute wheel or alternative?
35723. Why water is in liquid form
35724. Balancing and trading into words
35726. Finishing techniques for a steel motorcycle frame
35728. Fusable alloys
35729. Casting nickel
35731. SURSULF vs. TENIFER
35732. Online Purchase of AMS 2700 rev B
35733. WHAT IS THE ACCEPTED WAY OF DISPOSING OFCR-6 SOLUTIONS?
35737. Electroless Nickel plating on C14500 Tellurium Copper
35738. Preparation for brush nickel plating over damaged EN plating
35740. Process Capability of Adhesion Tape Test
35741. Yellow zinc chromate vs brass plating
35743. Aluminum in Clean Rooms
35748. Mirror finish on aluminum from burnishing or vibratory?
35749. "Spurs" - Tool for removing wax or compounding from buffer pad
35750. How does galvanized steel hold up to stainless in coastal environments?
35751. Slag resistance Black color coating on Zinc Alloy
35759. What are the reactions in acid tin fluoborate plating?
35760. Mechanical galvanizing
35769. Best way to prevent sterling silver from tarnishing in the jeweler's showcase?
35770. What process will deposit 300 series stainless onto copper alloy?
35772. Rust converter
35773. Ti Phosphate
35776. Re-Bluing Vs. Painting
35777. Hot-Dipped Galvanized Steel w/o Hexavalent Chrome
35778. Substrate hardness required before hard chrome?
35779. Internal plating of a cast iron engine water jacket
35780. Nickel Strike Cell concentration Breakdown
35787. Brightener for alkaline zinc-iron plating
35788. Removing chrome plating from cast bronze or brass
35791. Questions about TIN plating Magnesium electronic housings
35793. Zinc and Aluminum Plating on Aluminum Surface
35799. 5th grade Electrolysis / Electroplating Experiment
35800. Lemon, Penny, Rust
35801. Chemical film per mil-c 5541c
35803. To make gold, start with gold
35806. Cleaning my house AC condenser that has scale build up because of a leak at a faucet
35807. Would powder coating be appropriate for old claw footed tubs?
35808. International testing methods and standards for decorative plating
35809. Salt Spray Inspection by multiple operators
35810. Zinc Plating Specs and Hydrogen Embrittlement
35811. How can you test Alodine1200 solutions
35815. Titanium anode baskets suitable for cyanide zinc?
35816. What are the materials and equipment to be used in electroplating
35817. Ultra Flat Black Anodize - Specification?
35819. Setting up anodizing operation for job shop
35826. Electroplating from CuCl solution
35827. Where is the best place to buy a plating line, can it be done for under $10,000?
35832. Removing scratches from gold ring
35833. Porcelaining a cast iron pot
35834. Battery Acid on aluminum boat
35835. Is a brass bed affected by the humid weather conditions near the ocean?
35836. Bubbles on Plated Plastics
35837. Eliminating microcracks during chrome plating process
35838. How to go about non cyanide zinc
35839. Hard chrome on copper blisters at 130C
35846. ANALYSIS FOR SODIUM THIOCYANATE NEEDED
35847. Salt Spray Test Improvement, Waterbase Primer, Chromate Additives
35848. Nickel Plating on ZA-8
35849. Can your company re-chrome my rims...I have a Datsun 280 ZX
35851. I wish I could know what the ingredients were silly :-)
35853. Zinc types and their abundance
35855. World War II slate roofing
35858. Extracting elemental titanium from Titanium Dioxide
35861. What finish shall I ask for to get RoHS compliant zinc chromate?
35862. Resistance against sulfuric acid environment
35865. Spotting on Zinc Phosphated GI Sheet
35866. Excess nickel build up on nuts
35867. The problem about the internal stress in nickel sulphamate electroforming bath
35869. What is with the high Ni prices?
35870. Clear chromate conversion on zinc die casting
35871. Titanium anodic coating
35873. Degreasing of metal fasteners before shot blasting and dip spin coating
35879. Science experiment with zinc and sand
35881. Ni-Cd Electroplating process
35882. Specs for Black Anodizing of 6061-T6 Aluminum
35883. Anodizing female threads
35884. ALUMINUM GRINDING
35886. Carbon steel fasteners used on Duplex Stainless steel flanges
35890. Rust Deterrent for knives made from saw blades
35891. Health concerns, galvanized sheeting as bulletin board
35892. Testing after the passivation process
35897. How can I reduce the amount of Iron in my Cadmium tanks?
35898. Post nitric neutralization process
35901. Gold colored plating on motorcycle exhaust pipes and fork tubes
35902. Buffing out Etch marks in Clear Anodized Aluminum
35908. White stain/spot on annealed silicon steel
35910. Nucleus formation in solvent based coating in electrostatic coating
35911. Balanced Chemistry of Chrome Plating Bath
35912. Chrome plating on Inconel 718 material
35913. The correct finish process of Zamac3 Chromate conversion coating
35914. Need some practical Pictures of Defectives of Hard Chrome Plating
35915. Electroplating corrosion
35918. Anodic potentiodynamic, Tafel Lines, Cyclic voltammetry
35921. 420 stainless steel corrosion
35922. Salt spray testing: effect of conductivity of deionised water
35924. Discoloration from phosphorous bronze cleaning
35925. What to use to etch glass, stainless, plastic?
35927. Pinholing on external and internal radius
35928. Water Stains on Aluminum
35931. Chromate Properties
35934. Pre Galvanized Sheet instead of Hot Dip Galvanizing
35935. Electroplating
35936. Dark black and shining finish
35937. Black residue on IPA cloth wipes following passivation
35941. Corrosion
35942. New technology in fastener finishing
35943. Micro and Macro Etching Solution for Inconel 625
35944. Brass paint, heat resistant
35945. Aftermarket Chrome Rims peeling after small scrape
35947. Scrubber / Mist Eliminator for Acid Digestion
35951. Black Oxide Vs. E-coat
35954. Improving Laser Etch Contrast?
35955. Pickling Incoloy-800 (Stainless Steel)
35956. Permanent black finish for mild steel
35959. Refinishing a steel desk (stripping and applying new paint)
35962. Removing Phosphates from Wastewater
35964. How to present the Nickel Chrome Plating in International Standard
35968. Copper preservation
35971. Keeping diamond plate on fire trucks polished
35972. High temperature coating using metallizing
35974. Titanium anodic coating on anodizing racks
35975. DI vs distilled water for passivation immersion test
35981. 50 years old copper sulphate large crystal lumps from Germany
35983. Silverware Factory Experience
35984. Withstanding 500 hours of Salt spray to white corrosion
35985. Chemical Film, Mil-C-5541, on Aluminum-Vacuum Systems
35986. Phosphoric acid pickle
35987. Electropolishing vs electroetching (Dalic)?
35988. Need ultimate conductive coating
35991. Powder coating and RoHS
35992. How to calculate Cathode Efficiency in Chrome Plating
35997. Surface Mount Lead Corrosion