ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

Electroless Plating Compatible with Sulfur




2005

What other electroless platings are available?

I have found that Electroless Nickel works very well with rubber with cure systems other than a sulfur cure.

So, now I am looking for an electroless plating that is compatible with sulfur cured rubber.

Thanks,

Darrell Elkins
Manufacture of Rubber Products - Elgin, Illinois, USA



You might want to look at an immersion plating from a bath of Copper and Stannous sulphate with a ratio of 100:1

Khozem Vahaanwala
Khozem Vahaanwala
Saify Ind
supporting advertiser
Bengaluru, Karnataka, India
saify logo
2005



Khozem,

Thanks, I will check into copper and Stannous sulphate.

Darrell Elkins
- Elgin, Illinois, USA
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"