Poor adhesion of waterbased paint on acrylic solvent based primer coat



Dear,
I have encountered an adhesion problem when using waterbased coatings as topcoat on the dried acrylic solvent based undercoat on wood products. I really can not figure it out what was wrong with it. Could you help me in this matter

Thank

Best Regards

B Tan
Research - Enschede, The Netherlands
2005



I feel that the acralyic basic coating has to be little rough for your top coat of water based coating. Try roughing it with 00 emery paper lightly on a sample piece.

Many paints fail because of lack of adhesion.

SATYAJIT SHAH
- Mumbai, Maharashtra, India
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"