Electrocoagulation research




Dear Sir

I am a PhD student from Iraq. I have many difficulties in my research because of very difficult life in my country Iraq .My research is about using electro coagulation to remove heavy metals from waste water. Can you please help me by sending some case studies ,researches and any possible help.

Thanks in advance
Best regards

Suadmahdi
student - Hilla, Iraq
2005



One study was done as part of the EPA ETV pilot for metal finishing pollution prevention, the final report can be downloaded at: http://www.epa.gov/etv/pdfs/vrvs/06_vr_kaselco_fr.pdf

James Totter
James Totter, CEF
- Tallahassee, Florida
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"