ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

Need Expert Training in Electroplating Processes

adv.   robert probert banner 


RFQ: Hi, I am looking for a training place for chemical & mechanical aerospace electroplating testing. Please recommend a place that can provide it.

Adi sugiarto
Employee - Jakarta, Indonesia
August 30, 2023
    privately respond to this RFQ
Ed. note: As always, gentle readers: technical replies in public and commercial replies in private please (huh? why?)



⇩ Related postings, oldest first ⇩



Q. Hi,
We are looking for a web site or an organisation that help us to find expert in electroplating available to do training sessions in Tunisia.
I know that finishing.com is installed in United States, but I'm sure that you can help us.
Best Regards,

Adel HADDAD
Materials Engineer - Tunis, Tunisia
September 23, 2011


A. Hi, Adel.

You can check our Consultants Directory; some are geographically closer than the USA. You can also try Kushner Electroplating School and the National Association for Surface Finishing (nasf.ofg). There are organizations in England including the Institute of Metal Finishing, and the Metal Finishing Information Service. There is the Indian Association of Metal Finishers. Readers may have other associations and societies to suggest. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey


A. Hi Adel
The Institute of Metal Finishing in UK has a wide range of training courses leading to recognised qualifications in all aspects of metal finishing. These are available as distance learning modules.
There is a link from this website or go directly to

www.uk-finishing.org.uk/

geoff smith
Geoff Smith
Hampshire, England





(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"