Metal finishers helping each other -- No cost, No registration, No damn popups
(we earn from 'affiliate link' purchases, making the site possible)

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  Thread 342/23

Need mass finishing machine for valve plates, spring plates





Q. We are manufacturers of valve parts and spring parts. For the surface finishing we require suitable mass finishing machines. We require guidance from the experts of this machines manufacturers for achieving best results.

Mr.Manan
- Nasik, India
2005
publicly reply to Mr.Manan

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).



A. Valve plates and spring parts can be finished in mass finishing to achieve deburring at edges and polishing.

Many companies use this method but you would need a good supplier to suggest correct media and compound so that parts do not stick to each other.

PRASAD GOGATE
- Thane, Maharashtra, India.
January 8, 2018
publicly reply to PRASAD GOGATE



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"