Calcium Gluconate Gel for HF burns




RFQ: Dear Sir/Madam,

Can you tell me from where in India can we get Calcium Gluconate Gel as soon as possible.

We are in urgent requirement of the same for our Factory site, We would be grateful if you can provide us with some clue as soon as possible.

Thanks,

Vidisha M
medical technologies - Surat, Gujarat, India
2005

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).





similarly
Hydrofluoric acid burns left and right hands, two views, burned index fingers

Never use HF anywhere unless trained!
If you do, you MUST have the antidote gel on hand for instant use!


Calcium Gluconate
for HF acid burns

calcium_gluconate
on eBay or

Amazon

(affil links)

RFQ: Dear All,
Can you tell me where Calcium Gluconate Gel is available in India?
Regards,
Divyesh S
- Bharuch, Gujarat, India
August 12, 2008

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).





RFQ: Dear All,
Can we find/purchase Calcium Gluconate Gel in Indian market for our manufacturing plant?
Bablu D
- Kolkata, West Bengal, India
February 15, 2012

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).





RFQ: Can anyone guide me, where to find CALCIUM GLUCONATE GEL IN India.
Mugunthan
- Chennai,Tamilnadu, India
December 17, 2012

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).


A. Those who want calcium gluconate gel as safety item when working with the dangerous chemical ammonium bifluoride can now easily buy it by looking it up on the internet under its three letter name.

John Attard
San Diego, California, USA
2002


A. Hi. Yes, it is imperative (life critical) to have this on hand if you work with hydrofluoric acid (HF) !

Here are two brand names: Calgonate (www.calgonate.com) and Kays Medical (www.kaysmedical.com). We are not recommending or dis-recommending a particular brand, but after spending a lot of time googling myself, I think it would be worthwhile finding out if they ship to India. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey


A. I found this Indian company which could supply the HF Antidote Gel: Pyro Technologies (Bangalore) at www.pyrotechnologies.co.in
FYI

Satish Agrawal
Satish Agrawal
- Visakhapatnam, India
January 3, 2009


----
Ed. note: Their search engine says "no results found"; apparently you'll have to call to inquire

A. We are manufacturers of CALCIUM GLUCONATE GEL in India: www.southwestchemie.com

VASUDEVAN JAYARAJ
- CHENNAI, India
December 22, 2012


A. Dear All,
I have heard of a company in Delhi by the name Good Looks (India) that makes Calcium Gluconate gel. I long ago checked with their price and I think it is the cheapest compared to other brands that are very expensive. You may find the details about the company on google.com

Jizzi Nanda
- New Delhi, Delhi, India
April 3, 2014


... and posted from the same IP address the next day ...

A. CALCIUM GLUCONATE 2.5% GEL
If anyone is interested in getting Calcium Gluconate 2.5% Gel please contact me. I shall provide the needy in any quantity and at a very economical price.

Suresh Pujari
Chemical engineer - New Delhi, Delhi, India
April 4, 2014


----
Ed. note: "Price/demand curve for internet advertising: infinite demand at zero cost, zero demand at infinitessimal cost." -- Thomas J. Pullizzi, 1995



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"