What is Glow Bright #4





Anyone know what Glow Bright #4 is ?

Johnny McCaffrey
metal finishing - Houston, Texas
2004


----
Ed. note: Do we have any context, Johnny?



It's hard to give much wisdom on so little detail... but Glo-brite is an old trade name for a line of chemical products. Why do you ask?

Jeff Watson
Jeff Watson
- Pearland, Texas
2004


I am also looking for some information on Glo Brite #4. I am an engineer with an electropolishing company and we've had a request to use it or a similar product based on an older military spec. We can find nothing about Glo Brite. Anything regarding its chemical make-up, MSDS or similar products would be great. Thanks

Brandon LaBrozzi
- Lewis Run, Pennsylvania, USA
October 5, 2010



October 5, 2010

Hi, Brandon.

There is an Electro-Glo company in Lasalle, Illinois that specializes in electropolishing processes. I'd bet that Glo-Brite #4 is or was one of their products. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"