ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  Thread 232/32

BLACK OXIDE SPEC?




WHAT IS THE SPEC THAT CONFORMS WITH THE REGULAR BLACK OXIDE BATHS?

LUIS REBOLLEDO
- BROOKLYN, New York
2003
publicly reply to LUIS REBOLLEDO


See letter #531.

Ken Vlach [deceased]
- Goleta, California

contributor of the year Finishing.com honored Ken for his countless carefully researched responses. He passed away May 14, 2015.
Rest in peace, Ken. Thank you for your hard work which the finishing world, and we at finishing.com, continue to benefit from.

2003
publicly reply to Ken Vlach

Try AMS2485.

G. Grenert
- South Bend, Indiana
2003
publicly reply to G. Grenert

adv.
epi



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"