The below was a proposed technical program for an event and may not represent the final program, nor the contents of the Conference Proceedings for that event. If you are seeking a particular paper, contact the event's sponsor to make sure it is an actual part of their Conference Proceedings before ordering them.
INTERFINISH 96
14th World Congress & Exposition
International Convention Centre
Birmingham UK
10, 11 & 12 September 1996

INTERFINISH Technical Programme

TUESDAY, SEPTEMBER 10 1996
- 0900
- Opening Ceremony followed by Plenary Lecture - A general view, Nicholas V Scheele Chairman & Chief Executive, Jaguar Cars Ltd
Tuesday AM - 4 concurrent sessions
-
Session 1
- Paint Technology - 1
- Chairman: J Bernie
10.00
- Are we aiming at the right thing?
- R Pritchett, PRA (UK)
10.30
- Pairlt shop in the year 2000
- M Cowley, Ad-Qual (UK)
11.00
- COFFEE
- 11.30
- Life cycle engineering of painting technologies - Tool for optimisation and decision making.
- M Harsh, Institute forPolymer Testing and Polymer Science, University of Stuttgart (Genmany)
12.00
- Chromium free pre-treatment prior to painting.
- K Brown, Brent Europe (UK)
Session 2
- Engineering Coatings -1
- Chairman: Dr D R Gabe
10.00
- Investigation of wear in electrodeposited chromium coatings.
- N Martyak, K Newby, J McCaskie, Atotech (USA)
- 10.30
- Characteristics of electrodeposited chromium.
- M El-Sharif, C Chisholm, Glasgow Caledonian University
(UK)
- 11.00
- COFFEE
- 11.30
- The role of formic acid and methanol on speciation deposition rate and quality in the electrodeposition of chromium from trivalent electrolytes.
- S Ibrahim, A Watson, University of Paisley (UK) D Gawne, South Bank University (UK)
12.00
- Comparison of physico-chemical properties of Cr, Ni-P, Ni-Mo, Ni -W- P and Mn-Zn alloys coatings.
- T Agladze, S Bagaev, D Gabe, V Kudryavtsev, Ch Raub, S Schachameyer, N Spyrelis, T Tsupak. (Seven Universities World wide)
Session 3
- Zinc Alloys -1
- Chairman: Dr G D Wilcox
10.00
- Advances in replacements for cadmium plating in aerospace applications.
- K Baldwin, C Smith, Defence Research Agency (UK)
10.30
- The present status of zinc-nickel alloy coatings.
- S Watson, Nickel Development Institute (Canada)
11.00
- COFFEE
11:30
- Corrosion resistance of zinc alloy coated steel in construction industly environments.
- N Short, J K Dennis, Aston University (UK)
12:00
- Corrosion resistance of the plated Zn-Co alloy coating.
- T Zhenmi, Z Jingshuang, Y Zhelong, A Maozhong, L Wenliang,
Harbin Institute of Technology (China)
Session 4
- Management and Control -1
- Chairman: I R Christie
10.00
- Plating in a barrel, how does it work? A study of local mass transfer and current density distributions in a barrel.
- L Schuster, A Delvaux, M Degrez University Libre de Bruxelles (Belgium)
10.30
- Fully automatic on-line and off-line analysis for the plating industry.
- S Markl, G Strube, Max Schloetter (Gerrnany)
11.30
- Automatic control of deposited mass in hot dip galvanising.
- O Jacobs, University of Oxford (UK)
12.00
- Statistical process control in anodising using a personal computer.
- A W Brace, Consultant (UK)
----------------------
12.30 LUNCH
----------------------
Tuesday PM - 4 concurrent sessions
Session 5
- Paint Technology - 2
- Chairman: Dr A C Hart
14.00
- The challenge of powder coating car bodies.
- H Hofler, Gemma Volstatic (Switzerland)
- 14.30
- Advances in powder coating technology for automotive applications.
- G Bell, Courtaulds Coatings (UK)
15.00
- Performance of coated metal roofings and claddings.
- MOliver, BntishBoardofAgre'ment (UK)
15.30
- TEA
16.00
- Comparison of the multilayer polyolefin based system for the external protection of pipelines.
- P Perret, ElfAtochem (France)
16.30
- Corrosion protection of pipes, fittings and component pieces of water treatment and pumping stations.
- J Pey, ElfAtochem (France)
17.00
- The use of radiant heat transfer in the curing of coating on complex geometrics and problematic substrates.
- R Hampshire, Eastem Electricity (UK)
- Session 6
- Engineering Coatings - 2
- Chairman: B Wilson
- 14.00
- ACD deposition of diamond composites: relationship between phase composition and addition of surfactants.
- B Bozzini, G Giovannelli, F Ferrari, G Arman, G Bollini, L Nobili, P Cavallotti. Politecnico di Milano (Italy)
14.30
- Electrodeposition of composite layers consisting of inert inclusions in a metal matrix.
- K Helle, Akzo (NL), F Walsh, Universityof Portsmouth
(UK)
15.00
- Metal-oil composite plating for self lubricating bearings.
- S Matsumoto, S Jomjunyong, M Fujita Institute of Technology (Japan)
15.30
- TEA
16.00
- The effect of brush plating on the structure and wear properties of electrodeposits.
- J Gering, Institute of Materials (Gemmany), J P G Farr, University of Bimmingham (UK)
16.30
- Corrosion and wear protective composition modulated alloy coatings based on ternary Ni-P-X alloys.
- P Leisner, M Benzon, L Christoffersen, UniversityofDenmark
(Denmark), C Panagopoulos, V Papachristos, S Katsikis,
University of Athens (Greece)
17.00
- Corrosion behaviour of zirconium boron nitride and zirconium boride multilayer coated steels.
M Urgen, A Cakir, O Eryilmaz, University of Istanbul
(Turkey), C Mitterer, Institute of Metals (Austria)
- Session 7
- Zinc Alloys - 2
- Chairman: Dr J K Dennis
14.00
- Corrosion behaviour and mechanical properties of plated Zn-alloys.
- W Paatsch, W Kautek, M Sahre, Institute of Materials
(Germany)
14.30
- Electrodeposition and corrosion properties of zinc composite coatings.
- D Sneddon, M El-Sharif, C Chisholm, Glasgow Caledonian University (UK)
15.00
- Compositionally modulated zinc alloy coatings for corrosion protection.
- G Chawa, G Wilcox, D Gabe, Loughborough University of Technology (UK)
15.30
- TEA
16.00
- Zn-Mn alloy electrodeposition on steel.
- B Bozzini, G Bollini, P Cavallotti, Politecnico di Milano
(Italy) F Pavan, Pirelli (Italy)
16.30
- Functional composite zinc electrodeposition.
- A Sachian, M Blidariu, E Roman, C Raducanu ICTCM
(Romania)
17.00
- Plating from alkaline cyanide-free zincate baths.
- T Pearson, E Long, Wm Canning Ltd (UK)
Session 8
- Management and Control - 2
- Chairman: Dr D N Layton
14.00
- Multinational manufacturing giants to adopt QS 9000 type industry specific quality standard.
- P Pilplani, TTX Environmental (USA)
14.30
- Trends in electroplating in Japan.
- T Hayashi, University of Osaka (Japan)
15.00
- Quality finishing starts with Ser-Ductor agitation.
- C Reichert, Serfilco (USA)
15.30
- TEA
16.00
- The internet for INTERFINISH.
- K Umeda, K Kaminaga, Y Fukada, T Sato, Shibaura Technical University (Japan)
16.30
- The capability of industrial surface finishing processes to meet specifications.
- R Berglund, Swedish Institute of Production Engineering Research (Sweden)
WEDNESDAY, SEPTEMBER 11 1996
Wednesday AM - 4 concurrent sessions
- Session 9
- Paint Technology - 3
- Chairman: D Dasgupta
09.00
- New water based recyclable paint system.
- D Webber, Kemira Coatings (UK)
09.30
- Autophoretic coatings chemicals: a new technology to Europe.
- A Thomas, Henkel Metal Chemicals (Germany)
10.00
- An expert system approach to environmentally friendly finishing.
- R Kennedy, PRA (UK)
10.30
- COFFEE
11.00
- 'Intelligent paint'.
- N Whitehouse, A Doroszkowski, PRA (UK)
11.30
- Coatings for aero engine application.
- B Norton, Indestructible Paint (UK)
12.00
- Development and application of coil coated steel.
- B Jeffs, British Steel Strip Products (UK)
Session 10
- Academic Contributions -1
- Chairman: Dr J P G Farr
09.00
- Depth profile of composition in layered deposits with dual current pulses.
- K Hosokawa, Y Tsuru, N Misumi, M Matsunaga, Kyushu Institute of Technology (Japan)
09.30
- Characterisation of copper oxide layers by electrochemical methods,
- O Forsen, P Pesonen, J Aromaa, Helsinki University of
Technology (Finland) T Suortti Outokumpu Research
(Finland)
10.00
- The oscillation of an internal strain in Ni deposits under PR electrolysis.
- Y Tsura, T Tamai, K Hosokawa, Kyushu Institute of
Technology (Japan)
10.30
- COFFEE
11.00
- Electrochemical and spectroscopic studies of the influence of thiourea on the rate of copper deposition from an acid sulphate solution.
- S Campbell, E Farndon, F Walsh, University of Portsmouth
(UK) M Kalaji, University of Wales (UK)
11.30
- Kinetics of electrodeposition and properties of nickel-tungsten alloys.
- N Atanossov, M Bratoeva, Bulgarian Academy of
Sciences (Bulgana)
12.00
- Positron annihilation as a tool for characterising anodic layers.
- L Palffy, Coil Anodising and Coating (Belgium); H Schut, IRI (NL), D Segers, C Dauwe, T Hoecke. RUG
(Belgium)
Session 11
- Metal Spraying
- Chairman: Dr D R Eastham
09.00
- Thermal spraying -The future.
- K Harrison, Sulzer Metco (UK)
09.30
- Plasma spray deposition and engineering applications of magnesium hydroxide - polyamide composite coatings.
- Y Bao, D Gawne, South Bank University (UK)
10.00
- The microstructure of WC-Co coatings produced by HVOF spraying with liquid fuel.
- W Coulson, S Harris, University of Nottingham (UK)
10.30
- COFFEE
11.00
- Vacuum plasma spraying.
- K Scott, AEA Technology (UK)
11.30
- The influence of pretreatment on the adhesion of ceramic coatings on steel.
- D Gawne, B Griffiths, G Dong, South Bank University
(UK)
Session 12
- Automotive coatings
- Chairman: Dr J Edwards
9.00
- Decorative electroplating of plastics.
- A Hart Nickel Development InsUtute (UK)
9.30
- New methods of electroless plating and direct electroplating of plastics.
- A Vaskelis, E Norkus, G Rozovskis, J Vinkevicius, Institute of Chemistry (Lithuania)
10.00
- Corrosion resistance of the different coated steels for fuel tanks.
- L Storojeva, I P Bardin Central Research Institute
(Russia)
10.30
- COFFEE
11.00
- The corrosion resistance of Al-Mn alloy electroplated steel sheet.
- K Hirayama, J Uchida, A Shibuya, Sumitomo Metal Industries
(Japan)
11.30
- Some surface factors that affect the spot welding of aluminium.
- M Thornton, C Newton, B Keay, P Sheasby, Alcan International (UK) J Evans, University of Newcastle-upon-Tyne (UK)
----------------------
12.30 LUNCH
----------------------
Wednesday PM - 4 concurrent sessions
Session 13
- Autocatalytic Deposition
- Chairman: T Sato
14.00
- Electroless nickel plating of magnesium.
- W Fairweather, PMD (UK) Ltd (UK)
14.30
- The use of electroless nickel on automotive components.
- L Wing, Enthone-OMI (USA)
15 .30
- TEA
16.00
- Electrochemical techniques for the evaluation of porosity and corrosion rate for electroless nickel deposits on steel.
- C Kerr, D Barker, F Walsh, University of Portsmouth
(UK)
16.30
- Some properties of electroless Ni-P, Co-P, and Ni-Co-P deposits.
- J P G Farr, A Noshahi, University of Birmingham
(UK)
17.00
- New challenges for electroless plating technologies.
- J Hajdu, Enthone-OMI (USA)
Session 14
- Academic Contributions - 2
- Chairman: Dr V Kurdryartsev
14.00
- The coatings on nickel basis from low concentrated colloid-electrolytes.
- L Degtjar, B Dubov, I Kudrjavtzeva, F Kukos, State
Technical University of Novocherkassk ~Russia)
14.30
- Composite coatings - new insights leading to improved process control.
- J Celis, J Fransaer, Katholieke University of Leuven
(Belgium)
15.00
- High speed electroplating in low concentrated colloid-electrolyte baths.
- I Kudrjavtzeva, State University of Novocherkassk
(Russia)
15.30
- TEA
16.00
- Optimisation of the process of metal electrodeposition on highly porous cellular materials.
- V Kichigin, V Kamelin, V Antsiferov, O Koshcheev, Perm University (Russia)
16.30
- Microwave plasma enhanced CVD for high rate coatings of silicon oxide.
- O Takai, T Honjo, Nagoya University (Japan)
17.00
- Transparent water repellent films contained fluoro-alkyl functions bv RF Plasma enhanced CVD.
- A Hozumi, H Sekoguchi, N Sugimoto, O Takai, Nagoya University (Japan)
Session 15
- Aluminium Finishing
- Chairman: Dr A W Brace
14.00
- Improvements in the pretreatment of aluminium as a substrate for electrodeposition.
- T Pearson, S Wake, W Canning (UK)
14.30
- Mechanical etching of aluminium extruded products: an attractive and ecological process.
- W Barba, Italtecno (Italy)
15.00
- Surface treatments for enhanced wear resistance of aluminium.
- G Bokmark, IVF G Holmborn, L Granlund, IMC P Persson, Celcius J Siden, Ytema (Sweden)
15.30
- TEA
16.00
- Surface treatment of aluminium foam.
- K Kaminaga, K Toyoda, T Sato, Shibaura Technical University
(Japan)
16.30
- Electrocolour and other colours, titration, curves and electrolytic colouring bath for anodized aluminium.
- X Ventura, L C Syteme (Spain)
17.00
- Structural characterisation of nickel phosphorus cadmium coatings on aluminium connectors.
- N Martyak, J McCaskie Atotech (USA) W Richtering, M Larondelle, Atotech (Germany)
Session 16
- Environment - 1
- Chairman: Dr J P Celis
14.00
- Life after 1,1,1-trichloroethane - Options in vapour degreasing.
- G Howe, ICI Cleaning (UK)
14.30
- Assessment of surface cleanliness for metal surfaces using an electrochemical technique.
- M Baumgartner, Ch Raub, FEM (Germany) D Gabe,
Loughborough University of Technology (UK)
15.00
- Ultrasonic aqueous cleaning systems for the metal finishing industry.
- W Lambert, Kerry Ultrasonics (UK)
15.30
- TEA
16.00
- 'ACT-1' inerted alcohol based precision cleaning system.
- S Henly, Layton Engineering Ltd (UK)
16.30
- A new system for stainless drying of electroplated parts. The pulse blow drying process.
- A Mobius, LPW (Germany)
17.00
- Flameless thermal oxidation for odour control.
- J Young, D Wrightl Thermatrix (UK)
THURSDAY, SEPTEMBER 12 1996
Thursday AM - 4 concurrent sessions
- Session 17
- Environment - 2
- Chairman: Dr Muller
09.00
- A new approach to effluent treatment for the finishing industry.
- R Raiter, Adas Pty Ltd (Australia)
09.30
- The development of a novel electrochemical reactor for the removal and recovery of metals from waste streams.
- I Dalrymple, S Northcote, J Sutherland,EA Technology
(UK)
10.00
- Characteristics of micro-filters made of anodic oxide films of aluminium.
- S Hoshino, K Suzuki, K Nakane, Institute of Technology
(Japan)
10.30
- COFFEE
11.00
- Environmentally friendly stainless steel pickling.
- N Sanders, Solvay Interox (UK)
11.30
- Control of nickel emission in jewellery and related items.
- R Green, J Sargent, Engelhard-CLAL (UK)
12.00
- Alternatives for nickel in electroplating processes
- F Simon, Degussa (Germany)
Session 18
- Electronics - 1
- Chairman: Miss A H Chapman
- 09.00
- Optimising distribution in barrel gold plating.
- N Sawyer, ITT Cannon W Fairweather PMD (UK) Ltd
(UK)
09.30
- Formation of cobalt cyanide complexes in hard acid gold baths,
- R Green, T Jones, Engelhard-CLAL (UK)
10.00
- Testing of bright copper plating by rotating-cone electrode in PCB production.
- D Reichenbach, Ericsson-Nikola Tesla (Croatia)
10.30
- COFFEE
11.00
- Studies on the electrodeposition of ternary copper- zinc-tin alloys.
- W Miu, J Ross, F Lau, B Fong, Hong Kong Polytechnic University (Hong Kong)
11.30
- Lead free tin alloys as substitutes for tin-lead alloy plating.
- M Jordan, Max Schloetter (Germany)
Session 19
- Electroforming
- Chairman: R Parkinson
09.00
- Electroforming - a largely unrecognised but expanding vital industry.
- S Watson, A Hart, Nickel Development Institute (Canada)
09.30
- Precision electroforming using disposable plastic masters.
- C Barnes, T Crichton, Gilleffe Management (UK)
10.00
-
- Electroplated nickel in the manufacture of diamond tools.
- C Addison, 3M Ltd (UK)
10.30
- COFFEE
11.00
- Electrodepositionof alloys:improvementof properties in respect to electroforming.
- H Liebscher, W Muller, E Wachsmuth, Technical University, Limenau (Germany)
11.30
- Recent developments of electroforming with precious metals for jewellery.
- F Simon, Degussa (Germany)
Session 20
- Conversion Coatings -1
- Chairman: Dr W Paatsch
09.00
- Relationship in electrochemical properties, microstructure, industrial performance and salt spray resistance of passivators for white rusting of galvanised surfaces.
- D Singh, B Gaur, A Dey, National Metallurgical Laboratory
(India)
09.30
- Structure of zinc chromate coatings.
- N Martyak, J McCaskie, Atotech (USA) T Hulsmann, D Schroer, Atotech (Germany)
10.00
-
- Rare earth conversion coatings - A status report.
- A Hughes, K Nelson, CSIRO (Australia)
10.30
- COFFEE
11.00
- Chromium free metal pretreatment processes.
- W Roland, Henkel (Germany)
11.30
- Non-chromate conversion coating treatments for electrodeposited zinc-nickel alloys.
- J Wharton, G Wilcox, Loughborough University of Technology
K Baldwin, Defence Research Agency (UK)
12.00
- Study of conversion coatings on zinc deposition obtained from low pollution solutions,
- L Roman, M Blidariu, C Cristescu, ICTCM E Roman,
Chemical Research Institute (Romania
----------------------
12.30 LUNCH
----------------------
Thursday PM - 4 concurrent sessions
Session 21
- Late Papers
- Details to be announced at conference
- Session 22
- Electronics - 2
- Chairman: W Fairweather
14.00
- A new approach for the manufacturing of miniaturised pattern coils.
- T Daenen, M Hout, E Loenen, Philips (NL)
14.30
- Direct nickel plating on aluminium substrate for microbump formation.
- H Honma, H Watanabe, T Fujinami, Kanto Gakiun University
(Japan)
15.00
- Development of silver-cadmium alloy plating for electrical contact applications.
- M Mocofan, S Ivascun, M Preda, University of Craiova
(Romania)
15.30
- TEA
Session 23
- Coinage Metals
- Chairman: TBA
14.00
- Copper plating plant technology for coinage process design for waste minimisation.
- J D C Hemsley, Enthone-OMI. (UK)
14.30
-
- Technical challenges in the production of barrel plated coinage.
- M Rusco, Sherrit Inc (Canada)
15.00
- A novel chromising method for coinage applications.
- A Kempster, Diffusion Alloys (UK) P Hatherley, Royal Mint (UK)
15.30
- TEA
Session 24
- Conversion Coatings - 2
- Chairman: L D Brown
14.00
- Reactive coating metal pretreatment technology - The future?
- R Bridger, Walterisation (UK)
14.30
- Growing procedure for manganese-type chemical conversion coating for magnesium alloys and their adhesion with paint film.
- M Takaya, Chiba Institute of Technology (Japan)
15.00
-
- Molybdate based passivation of zinc.
- P Tang, G Neilsen, P Moller, Technical University of
Denmark (Denmark)
--------------------
15.30 TEA
--------------------
16.00 CLOSING CEREMONY - Presentation of Awards
- Preview of INTERFINISH 2000