Finishing Technology logo

"Finishing Technology Hotline BBS" Postings by Topic

Ed. note: before the internet existed, there was a time when "Sysops" (system operators) ran publics forums via dial-up modems and "BBS" (Bulletin Board System) software. Here is one such discussion from 1994.


Rinsing, Water, Waste Water Treatment



--------------------
Msg. #4482 in ** Ask Plater B**
Posted on 01/02/94 at 00:06:33
To: BERL STEIN From: VALENTINUS BRINKMANN - RINSING BERL, HOW CAN I GET A COPY OF YOUR PAPER ON RINSING? IS IT IN ENGLISH OR IS A TRANSLATION AVAILABLE?

--------------------
Msg. #4491 in ** Ask Plater B**
Posted on 01/03/94 at 08:03:36
To: VALENTINUS BRINKMANN From: BERL STEIN - Reply To 'RINSING'
Valentinus, three of my papers on rinsing came out in Metal Finishing, see the January '88, October '88 and July '89 issues. More papers were published in the USSR in Russian, but these three contain the most important material. Let me know if you have trouble finding the papers
- I'll send you copies. Cheers, Berl

--------------------
Msg. #4584 in ** Ask Plater B**
Posted on 01/12/94 at 23:15:57
To: BERL STEIN From: VALENTINUS BRINKMANN - Reply To 'RINSING'
THANKS BERL. BY THE WAY, I NOTICES AN ARTICLE ON CLOSED LOOP RINSING IN P&SF 8/93 BY MAX STEIN. ANY RELATION?

--------------------
Msg. #4586 in ** Ask Plater B**
Posted on 01/13/94 at 07:34:54
To: VALENTINUS BRINKMANN From: BERL STEIN - Reply To 'RINSING'
Hi, Valentinus, you guessed it right
- Max is my brother. We spent a lot of time discussing his approach, developing the model, etc. Cheers, Berl ----------------
Msg. #4594 in ** Ask Plater B**
Posted on 01/13/94 at 18:24:13
To: BERL STEIN From: TED MOONEY - Reply To 'RINSING'
That is a good article your brother wrote, Berl! /s

--------------------
Msg. #4626 in ** Ask Plater B**
Posted on 01/18/94 at 19:41:10
To: TED MOONEY From: VALENTINUS BRINKMANN - Reply To 'RINSING'
I SECOND THE SENTIM, VERY INTERESTING.

--------------------
 


Back to finishing.com Home Page Finishing Technology small logo