Metal microtubes






Q. Does anyone produce metal microtubes in materials other than stainless steels? I am looking at tubes that at: 0.020" ID 0.032" OD 0.006" Wall Sizes close to these dimensions would be OK too.

Thanks,

Subhasish Sircar
- Richmond, Virginia, USA
2001



What is the length? What are tolerances? What is the qty? Will Nickel be OK?

Payal Mag
- Charlotte, North Carolina
2001


A. Tubes like that can be produced via the electroforming process using either copper, nickel or nickel/cobalt.

Russell Richter
- Danbury, Connecticut, USA
2001




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"