Ross Miles Foam Height Test



Can anyone tell me what the official test method is for the Ross Miles Foam Height test?

Thank you,

Jennifer Bull
- Brampton, ON, Canada
2001



I need information about ross-miles foam test method.

Carlos Siller
DIKEN DE MEXICO - Saltillo, Coahuila, Mexico
2001



Q. I need the information about the Ross Miles Foam Test Method .

Ang Lai Cheng
- Johor Bahru, Johor, Malaysia
2001



A. The standard test method is ASTM D1173.
RFQ: Would you happen to know a supplier of the glassware required for this method?

Joe McCarthy
- London, Ontario
2002



I need information about ross-miles foam test method.
Thanks

Milena Ormastroni Menezes
- São Paulo, Brasil
2007



Q. DO YOU KNOW ANY OTHER STANDARD WHERE A FOAM FOR OIL IS EVALUATED, similar TO THIS TYPE OF STANDARD?

MONICA FERNANDEZ
- VENEZUELA
May 18, 2012




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"