ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

Satin Chrome




Q. Dear Metal finishers,

Have anyone heard of Satin Chrome? I've heard of Satin Nickel. Could it be Satin nickel plated with bright Chrome? If there is, are there any suppliers out there? Will appreciate very much if someone can comment on this.

Regards,

Jerry Huang
- Jakartar, Indonesia
2001



A. Dear Jerry:

It is possible to plate a follows to obtain Satin Chrome. Bright Nickel Undercoat. 4 to 5 microns. Satin Nickel - 7 to 10 microns Chrome plate at 10 ASF for 2 to 3 minutes. The finish will be smooth Non Reflective with a light blue tine.

Best of luck,

asif_nurie
Asif Nurie [deceased] [deceased]
- New Delhi, India
With deep sadness we acknowledge the passing of Asif on Jan 24, 2016



A. You can plate satin nickel directly on steel or copper. Bright nickel is a little bit risk. You can plate on satin nickel chrome, gold or brass. The look is very good.

Piotr Lobodziec
- Poland




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"