Clean Weld Discoloration on SST




We are looking for a chemical that will cleanup the weld bluing on stainless steel parts. We're not sure on the application process - paste or liquid. Any information in this area would be helpful.

Don Helder
GenMed Corp. - Grand Rapids, Michigan USA
2000



Hello Don,

We provide equipment to electrolytically remove heat tint from stainless steel weld areas. In addition the process will remove Ferrous corrosion and passivate the area to meet the requirements of QQ-P-35C (canceled) [link is to free spec at Defense Logistics Agency, dla.mil] and AMS2700.

Best regards,

Chris Helwig
- Valencia, California
2000




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"