  mfhotline


  -----

Want 3-phase-diagram for Al-Fe-Zn




Q. Dear all,
Can anyone give me a hint where I can find the Al-Fe-Zn 3-phase Diagram, preferably in the range between 300 and 500 °C (572 and 923 °F)?

Most suitable would be 350 °C (662 °F).

Many thanks in advance.

norbert seyfert
Dr. Norbert Seyfert
surface development - Olpe, Germany
March 2, 2014


A. Here are a few I can lend you. One diagram here is at 300 °C and another is at 450 °C. Sorry, I don't have 350 °C. Please see the 20 October 2012 edition of Journal of Phase Equilibria and Diffusion, Phase Diagram Evaluations: Section II by V. Raghavan.

blake kneedler
Blake Kneedler
Feather Hollow Eng. - Stockton, California
May 15, 2014




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"