  mfhotline


  -----

How to avoid resin marks in ED body





How to avoid resin marks in ED body? Although I have 3UF rinses and 2 DM rinses after ED, and many nozzles orientated, we cannot eliminate the resin dripping. Suggest me some ideas except spray orientation.

Sathish Agarwal
driving - Chennai, India
August 26, 2011



August 31, 2011

What exactly do you mean by Resin marks?
Can you publish photo?
It may help others also to understand.

Avinash Vidhate
- Nasik, Maharashtra, INDIA


Please check the solid content in your UF Rinse and DM Water rinse. Please maintain less than 0.5% solid level in final DM RINSE BATH AND MAINTAIN RINSING TIME,

Nithin reddy
- Bangalore, India
September 4, 2011




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"