Need Chrome Plate on Spring Ends




January 5, 2011

I am a spring manufacturer in Texas. The US government has a spring that needs to be chrome plated on the end coils only. Per Spec. SAE AMSQQC320 to a thickness of .0002-.0006.

Inconel x750 spring material.
Spring dimentions: .375 wire
OD: 3.25
Free Length: 1.75
53 parts

Is this something you could do?

Steve Hohman
spring manufacturer - Houston, Texas, USA




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"