ted_yosem
Sound technical content, curated with aloha by
Ted Mooney, P.E. RET
Pine Beach, NJ
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing since 1989
  mfhotline


  -----

Silver Master problem on polyester




December 2, 2010

We are having problems with the Silver Master on Polyester, no problem on glass. We have to use a lot of wetting agent on the PET or Polycarbonate to get successful shims. Our nickel sulphamate bath parameters are on target.

56266-1 56266-2

Any ideas? Could it be the Reducer, spray gun ratio?

Cheers

Alex Mag
Consultant - Sydney



December 22, 2010

Problem solved, please see the following link www.finishing .com/456/20.shtml

Cheers

Alex
- Sydney




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"