Cu/Ni 5b dark




Would anyone know the US finish equivalent of "Cu/Ni 5b dark" which appears to be a European plating spec. We are plating the material EN: CW614N (Europe)which is the equivalent of C38500 brass. I used the ASM International handbooks to find the US material equivalent but I am unaware of such a book for cross referencing finishes. Any ideas?

Mark Wright
manufacturing engineer - Rochester, NY, USA
February 11, 2010




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"