What kind of stainless steel is resistant to 93% sulfuric acid?




Good day! What kind of stainless steel resistant to sulfuric acid 93%?
(I need hose fittings for sulfuric acid 93% transportation)
Maybe 316Ti?
Thanks,

Jerry Fox
engineer - Finland
October 13, 2009


Better go for SS 316L

Kannan B
- Salem,Tamil Nadu, India
October 29, 2009




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"