Covering scratches and blemishes in Clear Anodizing




We received some clear anodized frame with minor scratches and blemishes. Is there a product available to take care of this aesthetic issue?

Thank you!

John Roberts
installer - Oklahoma City, Oklahoma
July 30, 2009



probertEthumb
Aluminum How-To
"Chromating - Anodizing - Hardcoating"

by Robert Probert

Also available in Spanish

You'll love this book. Finishing.com has sold almost a thousand copies without a single return request :-)


"The Surface
Treatment &
Finishing of
Aluminium and
Its Alloys"

by Wernick, Pinner
& Sheasby

pinner
(note: this book is two volumes)

on eBay or

AbeBooks

or Amazon

(affil links)

Hi, John. As long as there is no duplicity involved, use an indelible marker pen in a gray or silver color, as matches best. This isn't a joke; anodizing shops do it.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
March 13, 2010




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"