Pickling solution for removing oxide layer from Zr metal or Zr alloy





Dear Sir,
could you please let me know the composition of Pickling solution for removing oxide layer from Zr metal or Zr alloy.

Prashant S K
student - India
June 16, 2009



June 20, 2009

Try next solution:1 lit water/1 lit nitric acid/ 0,1 lit hydrofluoric acid! Be careful, use rubber rubber gloves this on eBay or Amazon [affil links] and safety goggles this on eBay or Amazon [affil links] ! According to M.Straschill: Neuzeitliches Beizen von Metallen (contemporary pickling of metals), Saulgau 1972.

Goran Budija
- Cerovski vrh Croatia




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"