Curing time for silver plating





Dear Sir,
We are using the silver plating in our organization Please tell me what is the curing time for silver plating.

Manoj garg
As QA I/C - Haryana
June 15, 2009



There is no curing time for silver plating, curing is associated with paints and adhesives, not plating.

So what do you really want? Is it the curing time of a silver loaded paint? Or is it the de-embrittlement time after plating that you require?

Brian Terry
Aerospace - Yeovil, Somerset, UK
June 18, 2009




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"