How to put #4 satin finish on aluminum pipe





I am looking a good way to blend a #4 satin finish on aluminum

Jeff Hennequin
shop foreman - Queenstown, Maryland
May 20, 2009



First of two simultaneous responses --

Dear sir

Use glass bead blasting.

Suresh Reddy
- Bangalore
May 26, 2009



Second of two simultaneous responses --

How long are the tubes? What is the I.D.? How many parts /hr.? If they are longer than 12 inches you are probably better off with a non-woven wheel pass through system.

tony kenton
AF Kenton
retired business owner - Hatboro, Pennsylvania
May 26, 2009




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"