Stripping agent for powder coats





February 23, 2009

Experts,
Would you please name some stripping agent useful for cleaning the surface free from electrostatic powder coat on passivated aluminium die cast component. Please also comment about the influence of powder coating method (Spray method / Fludized bed method) and time-span between post-curing of powder coats and its removal by stripping.

Thanks in advance!

Kasi Subbiah Perichiyappan
surface treatment engineer - Bangalore, Karnatka, India


I would assume that tech services for the OEM paint company could provide you with some guidance or recommend a paint strip vendor.

James Watts
- Navarre, Florida
February 25, 2009




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"