Microwave oven for baking e coat





February 11, 2009

Our company is in the process of installing an E-Coat facility and we have plans for including a LPG-fired convection type oven for baking.
I recently read about microwave type ovens that are available for industries.
What do you think will be the most striking advantage and limitation?

Kaushik Ram
Plating shop employee - Pune, Maharashtra, India


Apart from the feasibility of heat control my biggest worry would be the H & S aspect of the system... we have all read about the dangers to our eyesight due to loose fitting doors on domestic MW ovens. But I await to be corrected.

Terry Hickling
Birmingham, United Kingdom
February 13, 2009




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"