Sn Plating Looks Like Zn After Autoclave Test




September 20, 2008

We submitted some Microelectronic samples to AutoClave testing (96 Hs.) and when we removed the samples an oxidation formed on the surface of the leads and the body of the parts that looks like Zn plating! Has anyone observed this condition before, and can you tell me what was responsible?

50043-1

50043-2

Chris MacMartin
Failure Analysis - Simi Valley, California, USA



Let's dip out a 4 liter beaker [beakers on eBay or Amazon [affil links] , dummy out the copper, carbon treat with powdered activated sulfur free carbon, then plate a part in the beaker and see if it corrodes in the autoclave. Let us know.

robert probert
Robert H Probert
Robert H Probert Technical Services
supporting advertiser
Garner, North Carolina
probertbanner
September 22, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"