Metal finishers helping each other -- No cost, No registration, No damn popups
(we earn from 'affiliate link' purchases, making the site possible)

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

Stainless fasteners to be used poolside ?




HI WE ARE A FASTENER COMPANY IN ENGLAND WHO HAVE AN ENQUIRY FOR STAINLESS FIXINGS TO BE USED FOR FASTENING HANDRAIL AROUND A SWIMMING POOL. CAN WE SUPPLY A2 OR A4 NUTS & BOLTS
OR WILL THE ATMOSPHERE CAUSE RUSTING TO APPEAR ON THE BOLT HEADS OR DOME NUTS.

MARK SHEPHERD
FASTENER DISTRIBUTOR - NEWCASTLE, ENGLAND
June 24, 2008



Alloy 316 is best for pools.

don baudrand
Don Baudrand
Consultant - Poulsbo, Washington
(Don is co-author of "Plating on Plastics" [on Amazon or AbeBooks affil links]
           and "Plating ABS Plastics" [on Amazon or eBay or AbeBooks affil links])
June 27, 2008


Agreed, 316 is recommended and electropolish the fasteners also this will GREATLY increase the corrosion resistance.

Cliff Kusch
electropolishing shop - North Vancouver, British Columbia, Canada
September 21, 2009




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"