How to remove fusion glued logos from our ionized aluminium cameras?




We had our logo glued by fusion on our black ionized aluminium cameras (silk screening). How do we remove the logo without damaging the aluminium?
Thank you for answering with your tips or a product we can buy for the removal.

Jennifer Boulanger
- Sainte-Adele, Quebec, CANADA
June 23, 2008



My guess is that you would probably need to paint over the logo and then silk screen another logo on it. By ionized, I assume that you mean anodized and black dyed.
The paint has at least partially gone into the anodize, so mechanical removal means will not work. Chemical methods are nasty and would probably damage the dye.

James Watts
- Navarre, Florida
June 25, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"