Plating on a high chrome surface



We are in the pogo pin industry. Can we hard chrome a pure copper plate and then plate another layer of silver as we need a hard surface and yet to be able to have a high electricity flow ( Doing resistance testing on our pogo pin after a few thousand cycling). We experiencing high wear and tear on our current design plate (pure copper plated with Ni then Silver)

Mike Tan
Electronic - Singapore
June 20, 2008



Hi, Mike. I don't know if that is practical or not. But what is very practical is electroless nickel (also very hard surface) followed by silver.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
June 23, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"