The process for electroless nickel plating




June 20, 2008

dear sirs,
I am Hanifa Khan from India... with submission intend to get from you the processes for electroless nickel plating. I have already got some informations about it but those are not sufficient.
so sir please help.

Hanifa Khan
general manager - Durgapur, WB, India



June 24, 2008

Hanifa,

If you search the literature and/or patent information you will find formulations for an older class of generic baths. These will be lacking in rate, stability and quantity of metal turnovers. By working with this information, you can develop a bath. However, what you will have developed will be old technology since deposits from the bath will not meet ROHS requirements or many others which severely restrict heavy metals.

I think that you should contact a local supplier of plating chemistry and see what they have to offer.

Gene Packman
process supplier - Great Neck, New York




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"