What showerhead won't rust or corrode quickly




I am lookng for a shower head as the last one rusted quickly.
My choices are brass, chrome, or pearl platinum.

Which metal is least likely to rust? Also, refrigerators in Hawaii rust in record time on the doors. Does anyone know if they make a rust resistant frig.

Aloha,
Shannon

Shannon Cormie
student - Kona, Hawaii
May 6, 2008


Aloha Shannon. I think what you need is a showerhead that is actually made of brass, regardless of what color it is painted or plated. Hunt for a solid brass showerhead and it will hopefully be your last.

Most modern refrigerators have heating coils in the door and a switch to turn them on or off. The heating coils keep the door dry. Otherwise the door is cool and moistures condenses on it. It costs energy to use the heating coils, but the door will rust in a humid climate if you don't.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
May , 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"