Recycling used aluminium printing sheets




April 16, 2008

I have a daily stock of used aluminium printing sheets and would like to dispose it off.
Is there any profitable means of doing the same or by reprocessing it?
thank you

Vasi Shaikh
employee - Jeddah, Saudi Arabia



Vasi,
Perhaps your Al sheet supplier has the means of re-processing the Aluminum and can issue you a credit for the amount you ship to them. If not, a local scrap yard will pay you for it.

Mark Baker
Process Engineer - Syracuse, New York
April 20, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"