ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

Usage of SS316 material in purified water distribution loop




March 9, 2008

Is it compulsory to use SS316L in Purified water distribution loop.
Does it impact the quality of water by using SS316 material piping.

Krishna Bala
pharmacutical industry - Hyderabad, Andhra Pradesh & India



First of two simultaneous responses --

The L is for low-carbon, which improves welding properties. Water quality will not be affected.

ray kremer
Ray Kremer
Stellar Solutions, Inc.
supporting advertiser
McHenry, Illinois
stellar solutions banner
March 28, 2008



Second of two simultaneous responses -- March 30, 2008

Dear Krishna Bala
it is not compulsary to use ss316l in purified wTER DISTRIBUTION Loop you can use ss304L also because ss316L better resistance to acidic atomaspher.in Purified water distribution loop is not must I think.

Umashankar Gupta
- Hyderabad




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"