Is Ebonol non-conductive?




Does Ebonol make copper electrically non-conductive? If it does where can I get it?

Anita Oliver
hobbyist - Tallahassee, Florida, USA
2007



First of two simultaneous responses --

Anita,
Are you are referring to Ebonol C, a copper oxide formulation made by Enthone-OMI? Copper oxide is non conductive, but it would depend on the application and the end use to determine how long the treated surface would remain non-conductive. Check with the experts. I have also heard of Ebonol on string instruments, which I think is entirely different.

Mark Baker
Process Engineer - Syracuse, New York
2007



Second of two simultaneous responses --

Try www.ethone.com website.Probably Ebonol C coating is sulfide based-in that case it is (probably) just somewhat less conductive than pure metal. Hope it helps and good luck!

Goran Budija
- Cerovski vrh Croatia
2007



Dear Anita,

The ebonol c is a product based on very strong oxidizers between highly alkaline itself is non conductive

Hernan Zalio
apholos - Buenos Aires, Argentina
March 26, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"