What is E512 per MIL-F-14072

none
finishing.com is made possible by ...
this text gets replaced with bannerText
spacer gets replaced with bannerImages


Q. What is E512 per MIL-DTL-14072 [⇦ this spec on DLA]?

Larry Davila
qa manager - Gardena, California
2007



probertEthumb
Aluminum How-To
"Chromating - Anodizing - Hardcoating"

by Robert Probert

Also available in Spanish

You'll love this book. Finishing.com has sold almost a thousand copies without a single return request :-)


A. See MIL-DTL-14072E Finishes for Ground Based Electronic Equipment, page 44:

TABLE IV. Finishes or processes other than painting or plating (E) - continued.
For Use On: Aluminum alloys when Low Resistance Electrical Contacts are required; service temperatures not to exceed 60 °C

Type Exposure: II

Finish Number: E512

Finish Process: 1) Preconditioning not required.
2) Passivate with chemical film per MIL-DTL-5541 [⇦ this spec on DLA], Class 3.

Ken Vlach [deceased]
- Goleta, California
contributor of the year Finishing.com honored Ken for his countless carefully researched responses. He passed away May 14, 2015.
Rest in peace, Ken. Thank you for your hard work which the finishing world, and we at finishing.com, continue to benefit from.





(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"