  mfhotline


  -----

Phosphating fails salt spray test




My phosphatnig solution doesn't withstand for salt spray test of 24 hrs.
I want it to withstand for atleast 48 hrs.this is main part of my project.
which chemicals along with H3PO4 should be added ?
The aim of my project is to protect mild steel for 48 hours or more...
please help me.

Sagar Deshpande
student - Alibag, Satara, Maharashtra
2007



2007

Hi

You can apply any good rust preventive oil after phosphating to meet your requirement.

Regards,

Anurag Kanaujia
A- New Delhi




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"