Metal finishers helping each other -- No cost, No registration, No damn popups
(we earn from 'affiliate link' purchases, making the site possible)

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  Thread 452/87

Refinishing outdoor aluminum furniture




I have a set of aluminum outdoor furniture (Brown-Jordan) that I would like to refinish. Can someone recommend the steps we should follow?

Brian Miles
Consumer - Fenton, Michigan
2007
publicly reply to Brian Miles


Hi, Brian. Although it's obvious to you what you are dealing with and what you want, it's not obvious to we readers. Is this painted aluminum that you wish to repaint, or bare aluminum that you wish to re-polish, or bare aluminum you wish to paint? Are all non-aluminum parts removed? Thanks.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2007
publicly reply to Ted Mooney


Glass bead blast to remove all old paint and corrosion, then prime and paint with automotive-quality materials. Any store which sells auto paint can supply you with the correct primer and topcoat.

jeffrey holmes
Jeffrey Holmes, CEF
Spartanburg, South Carolina
2007
publicly reply to Jeffrey Holmes, CEF



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"