Please Help me for chemical black finishing (hot and cold)




2007

Dear All,
I live in Iran. I want to know the procedure of Chemical Black Finishing ( Hot & Cold ).
Can every one help me?. I want to know :
1: which material and which chemical material I must use for chemical black finishing ?
2: the equipments and instrument I must use.
3: procedure from A to Z.
4: procedure of matte and glass chemical black finishing.

With the best regards
Hossein

Hossein Mohammadzehi
gunsmith - Iran



We have a FAQ about hot and cold blackening on line here, Hossein. Beyond that, move to the Metal Finishing Guidebook for further detail. But complete A-Z knowledge will come only from years of experience. Also note that hot blackening is very hazardous. Your best best is to align with a supplier who offers a proprietary solution. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2007


adv.
epi



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"