Instead of iodometric titration for copper analysis in electrolyte, any other methods available or not




Now we are doing copper (gpl) analysis by iodometric titration in electrolyte .is their any other methods available for copper (gpl) analysis other then iodometric method.

B.Mariappan
technician - Tuticorin, Tamilnadu, India
2007


ICP and you will be able to do other dissolved metals as well

Terry Tomt
- Auburn, Washington
2007


If you need to only know total copper, than I definitely agree that ICP is the way to go. If you need to differentiate between species of copper, and Ion Chromatograph is beneficial.

Jennifer Friesen
- Winnipeg, Canada
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"