Effect of silicon steel on efficiency of small electric motor




We are produce small electric motor which used in refrigeration compressors and now we are using the magnetic steel without silicon and to increasing the efficiency of our product we need to used silicon steel instead of steel without silicon steel
If any body have more information about the different between the magnetic steel with/without silicon , more thanks

Fawzy Elberembaly
R&D Manager - Cairo, Egypt
2007



Hi there,
There has to be an insulator of some sort between the laminations, or the motor will overheat.

Ken Foyn
- Durban, South Africa
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"