Conductivity of Zinc Cobalt Plating




Can any one give accurate conductivity comparisons between olive drab cadmium and zinc cobalt as a finish plating.
Opinions seem to differ on this point and I would appreciate informed views.

A P O N T I N G
Aerospace Industry Employee - Cheltenham
2007



Hope this helps you.
Cadmium has a conductivity of 1.462E+07 siemens/m
Zinc-cobalt - 1.670E+07 siemens/m (depending on the exact alloy plated)
Pure silver - 6.287E+07 siemens/m (provided as an example)
The Zn-Co alloy would have a higher conductivity rating.

Mark Baker
Process Engineer - Syracuse, New York
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"