Corrosion resistance for electroless tin plating?




I am now coating small component by electroless tin plating in barrels. I would like to know how to prolong the corrosion resistance for the tin coated components. Please let me if there are any lacquers or other process to resist corrosion.
Thanks,

Dinesh Samuel
plating products - Bangalore, India
2007



Dinesh Samuel

Better you specific the salt spray hours.
Normally tin plating will help for electrical contacts.
Better you do some organic lacquers /Sealants after plating.
It will help you little bit.

Kannan Boopathi
- Bangalore
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"