Peroxin test used in electroless nickel plating




I am doing high phosphorus electroless nickel plating process on EN series metal jobs with sand blasting as the pretreatment.I want to know whether there is any test named as Peroxin test used to check the plated components. Can I please get the details of this test.

Shailesh Agashe
Plating Shop - Pune, Maharashtra, India
2007



I am not familiar with it, but please tell us why you think there is such a test -- and what the test is used to test for -- and maybe we can help you track down something useful. Perhaps something to do with peroxide, but I suspect that the situation involves using the EN in some sort of Peroxin processing context rather than being a more general type of test. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2007



First of two simultaneous responses --

Closest thing that I can think of would be a Feroxyl test for complete plating on iron.

James Watts
- Navarre, Florida
2007



Second of two simultaneous responses --

I have not heard of any such test for EN either. As far as I know peroxin refers to proteins in genetic profiling. Could you have the name of the test confused with something else?

Mark Baker
Process Engineer - Syracuse, New York
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"