Chrome-like sputtering on aluminum alloy wheels




2006

Dear Sirs,
I need help to select a sputtering system for aluminum alloy wheel that will give shiny effect like chrome and good bonding.
Please help.
Thanks

Hin Teo
- Singapore



Why don't you plate real chrome on your alloy wheel?
Appearance , adhesion and corrosion resistance of real chrome are better than sputtering. From the case of two wheel brands in Malaysia , both had produced chrome-like colour with sputtering system.
They were claimed from customer very much because sputtering layer peeled from wheel.
Nowadays these two companies have only real chrome wheel for selling .

Aon Dum
electroplating - Thailand
2007


If sputtering is processed in the right way, with the whole right procedure of preparation and finishing, is much better in terms of resistance than electroplating; I can give more information.

Antonio Kolzer
- Milan, Italy
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"