ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

CORROSION RESISTANCE CHART FOR HASTELLOY




2006

Dear sir,

For plate type sea water cooler, what are the disadvantages of using HASTELLOY for plate material.

The sea water temperature is 32 deg C.

The maximum temperature of the liquid for cooling is 90 deg C.

Similar cooler will also be used for condensing propane/Butane gas. Maximum gas temperature 130 °C. Condensing temperature is 32 °C.

Appreciate if I could get corrosion resistance chart for HASTELLOY and titanium.

is a comparison table for above 2 material is available?

Best regards,

Ramesh Kumar
Ship manager - Mumbai, India



2006

For data on the various HASTELLOY® alloys, see the manufacturer's website: http://www.haynesintl.com/

For corrosion data on titanium, see Timet's document: http://www.timet.com/pdfs/corrosion.pdf

Ken Vlach [deceased]
- Goleta, California

contributor of the year Finishing.com honored Ken for his countless carefully researched responses. He passed away May 14, 2015.
Rest in peace, Ken. Thank you for your hard work which the finishing world, and we at finishing.com, continue to benefit from.





(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"