Passivation of aluminum alloy



Dear Sir;
I would like to know how aluminum alloy passivate.
Thank you in advance for your assistance

I am looking forward to receiving your reply
Yours Sincerely
Amen

Amen Ahmed
Oil Company - Zawia, Libya
2006
publicly reply to Amen Ahmed


Hello, Amen. "Surface Treatment and Finishing of Aluminum and its Alloys" should give you a full appreciation of this subject. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2006
publicly reply to Ted Mooney



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"