Can you colour platinum




Hi I'm a level six jewellery student and was wondering if anyone knows if you can colour platinum at all.

Sarah Roston
trainee jeweller - Sheffiled, South Yorkshire, U.K
publicly reply to Sarah Roston

Try black platinum plating, or black rhodium [adv: black rhodium plating solution on eBay or Amazon [affil links] or even nickel. Hope it helps and good luck!

Goran Budija
- Cerovski vrh Croatia
2006
publicly reply to Goran Budija


Platinum cannot be colored. Black platinum is caused by improper plating techniques and the platinum bath is thereby completely ruined.

blake kneedler
Blake Kneedler
Feather Hollow Eng. - Stockton, California
2006
publicly reply to Blake Kneedler



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"