Please suggest jet black colour with coating other than DLC




Possible to get using TiN ,TiC at 0 bias voltage? this will help for my research. I am junior research fellow doing on decorative coatings.

plaese help me.

angadala, PVD coatings engineer
- Pune, Maharastra, India
2006



Hi Murri,

How do you Decorative coating? DO you do that with Plasma Vacuum Deposition Method ?

Murthy
- Hyderabad , India
2006



Dear Murthy,

I will do with PVD arc process. can we get jet black colour .if you have any idea please let me know.

angadala, PVD coatings engineer
- Pune, Maharastra, India
2006




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"